# Cracks and crack-like defects

In short. Why metal-loss formulas do not apply, what §192.712 requires of a crack analysis, and how the gas and liquid schedules differ today.

A crack fails by fracture or by fatigue, not by the bulging of a blunt ligament. ASME B31G and its modified form have no term for toughness and no term for a sharp tip. Putting a crack depth into the metal-loss calculator on this site will produce a number and it will be the wrong number. The calculator is labeled for blunt metal loss for that reason. There is no crack calculator here, because a responsible one needs a fracture-mechanics model, a toughness that belongs to the pipe, and a loading history. A single-screen tool would pretend those are optional.

[Section 192.712(d)](https://www.ecfr.gov/current/title-49/section-192.712) states the gas-transmission duty. The predicted failure pressure comes from a model appropriate to the failure mode (ductile, brittle, or both), the pipe and weld properties, and the way the flaw was sized. If the segment sees cyclic fatigue or another crack-growth mechanism, the operator analyzes growth — Paris-law fatigue is the example the section itself gives — and defines remaining life as the time for the crack to grow to the size that fails at MAOP. That life is re-evaluated before half of it expires. Where toughness is not in traceable, verifiable, and complete records, the conservative Charpy values in §192.712(e) are the ones the section requires, not a generic upper-shelf number. Pressure-test results can bound the largest crack that could have survived the test; they do not measure the crack that is there.

## Schedules in force

After the January 2025 correction, the immediate gas criterion that used 1.25 times MAOP for cracks is gone. PHMSA’s 2026 proposal describes what remained: an immediate response when crack depth reaches 50 percent of the wall, and no failure-pressure immediate criterion until a new rule creates one. The proposal would set the immediate failure-pressure ratio at 1.1 and move the immediate depth threshold to 70 percent, with 50 percent becoming a near-term condition. Those are proposed numbers. The current eCFR text of §§192.714 and 192.933 is the list that applies, including whatever one-year and monitored crack conditions those sections still contain beyond the immediate list. Do not manage cracks on a summary.

Liquid integrity management still treats a crack that is confirmed when the indication is excavated as a 180-day condition under [§195.452(h)](https://www.ecfr.gov/current/title-49/section-195.452), and it does not have a federal failure-pressure crack criterion yet. The 2026 proposal would add one, at a ratio of 1.1 for immediate response and 1.39 for near-term, plus depth thresholds. API RP 1176 is the consensus recommended practice the proposal cites. It is not today’s incorporated schedule.

## Colonies, seams, and coatings

Stress corrosion cracking arrives as a colony, not as a single tidy crack. Length for a fracture model is the length of the interacting colony, which is a technical judgment, not the longest individual crack the tool called. The Marshall report is the public demonstration of colonies under disbonded polyethylene tape growing by corrosion fatigue until they linked. A repair that sleeves one crack and leaves the colony, or recoats with the same shielding tape, has not addressed the condition the investigation describes.

Selective seam weld corrosion behaves like a crack because the seam is the crack starter. The gas rules pull some of those seams into the immediate metal-loss list at a failure-pressure ratio below 1.25, using a fracture model rather than ordinary B31G. High-frequency ERW was removed from that immediate list by the 2025 correction. Vintage low-frequency ERW, direct-current ERW, and flash-welded seams were not given a clean bill of health by that removal. Pre-1970 LF-ERW, the wide heat-affected zone, and the assessment method [§195.452](https://www.ecfr.gov/current/title-49/section-195.452) requires for that seam are on the [LF-ERW note](/assessment/lf-erw-seams/).

Grinding out a shallow crack and proving the tip is gone can be a repair, within the limits on the [grinding note](/repair-methods/grinding-and-recoat). A crack that is long, deep, or in a low-toughness seam is a cut-out. Covering it is not an analysis.

## Longitudinal cracks and circumferential cracks are not the same repair

A longitudinal crack is opened by hoop tension. The 2021 PRCI repair manual treats a steel compression sleeve — a Type A sleeve installed so the carrier under it stays in hoop compression — as a way to take that tension off SCC and similar crack-like defects. The same manual says that sleeve is the wrong object for a circumferential crack and for a defect in a field bend. Circumferential stress-corrosion cracking and a weak girth weld are opened by axial tension. Pressure-only tests do not qualify a repair for that load.

A 2026 full-scale program, IPC2026-185396, tested composite sleeves and steel compression sleeves on machined circumferential grooves, 40 to 80 percent through-wall, in 12-inch and 24-inch pipe, under pressure plus axial tension. Both non-welded systems increased stiffness and axial capacity relative to the unrepaired groove. Type B sleeves, welded to the carrier at the ends, went further: those specimens failed in the pipe body rather than at the groove. The non-welded repairs still lost containment at the groove. The program also found that a repair installed at a pressure below the field installation pressure will look stronger in the lab than it will be in the ditch, because later pressurization adds radial compression the field bond never had. Details and the citation are in the [research summary](/research#ipc2026). Nothing in that program amends §192.712 or §195.452. A crack repair is still a fracture-mechanics problem plus a method the rule actually allows.

## Sources

- [49 CFR 192.712(d)](https://www.ecfr.gov/current/title-49/section-192.712) — eCFR
- [49 CFR 192.714 and 192.933](https://www.ecfr.gov/current/title-49/section-192.933) — eCFR
- [2025 correction removing the 1.25 MAOP crack trigger](https://www.federalregister.gov/documents/2025/01/15/2025-00073/pipeline-safety-safety-of-gas-transmission-pipelines-repair-criteria-integrity-management) — Federal Register
- [49 CFR 195.452(h)](https://www.ecfr.gov/current/title-49/section-195.452) — eCFR
- [NTSB/PAR-12/01, Marshall](https://www.ntsb.gov/investigations/AccidentReports/Reports/PAR1201.pdf) — NTSB
- [2026 NPRM, crack response discussion](https://www.federalregister.gov/documents/2026/07/08/2026-13805/pipeline-safety-repair-criteria-for-hazardous-liquid-and-gas-transmission-pipelines) — Federal Register
- [API standards catalog (RP 1176 is listed there)](https://www.api.org/products-and-services/standards) — API
- [PRCI catalog, Updated Pipeline Repair Manual, 2021 Edition](https://research.prci.org/Research/DesignMaterialsConstruction/DMCProjects/MATR-3-1A/186889/235745.aspx) — PRCI