title: "Composite sleeve repair of a dent and seam-weld crack on a 24-inch crude-oil pipeline"
description: "Non-welded pre-cured composite reinforcement of a dent and ground-out seam-weld crack on a 24-inch X52 crude pipeline."
section: case-studies
updated: 2026-11-25
canonical: https://pipelinerepairs.com/case-studies/cs-13-composite-sleeve-repair-of-a-dent-and-seam-weld-crack-on-a-24-inch-crude-oil/
markdown: https://pipelinerepairs.com/articles/case-studies/cs-13-composite-sleeve-repair-of-a-dent-and-seam-weld-crack-on-a-24-inch-crude-oil.md
---

# Composite sleeve repair of a dent and seam-weld crack on a 24-inch crude-oil pipeline

In short. Non-welded pre-cured composite reinforcement of a dent and ground-out seam-weld crack on a 24-inch X52 crude pipeline.

Source: CSNRI / Critica Infrastructure (Clock Spring). Account type: Vendor account.

An onshore 24-inch X52 crude line had a dent and a crack in a seam weld. The operator wanted to avoid welding and had already looked at a carbon-fiber wrap, which it considered too slow and costly. The line was taken out of service but left full while technicians ground out the crack, filled the dent, and installed two pre-cured composite sleeves by hand spool. CSNRI says two local technicians finished the installation in about four hours. As with other manufacturer case studies, the performance and cost comparisons should be read as the vendor's claims.

## Method

Crack ground out, dent filled, then two standard 24-inch Clock Spring composite sleeves installed by the hand-spool method, plus a single-wrap mold and two filler kits

## Defect

Dent with a crack in the seam weld

## Pipe

24-inch (610 mm) carbon steel API X52 crude-oil pipeline, onshore (technicians described as coming from the Netherlands). Operating pressure not stated. The line was taken out of service but not evacuated during grinding.

## Outcome

CSNRI reports two technicians finished the sleeves in about four hours, with no welding, and describes the work as about 25 percent of the time and 35 percent of the cost of an alternative (unspecified) solution, with a 50-year validated service life. Time, cost, and life claims are the vendor's.

Schedule, cost, and service-life figures in this note are the publisher’s claims. They were not checked against an operator record or a laboratory report.

Dates: Year not stated.

Maker named in the source: CSNRI (Clock Spring).

## Sources

- [Clock Spring repair of a dent and seam-weld crack on a 24-inch crude-oil pipeline](https://www.cs-nri.com/case_study/clock-spring-repairs-24-inch-crude-oil-pipeline/) — CSNRI / Critica Infrastructure (Clock Spring)