# Compression sleeve on a crude line, Middle East operator

In short. A shop trial and a first live compression-sleeve install, taken from a forthcoming conference paper. The operator is not named because the paper is not in the public proceedings.

Source: forthcoming conference paper (2026). The draft is not hosted. A search of the public IPC 2026 proceedings on 25 November 2026 did not find this paper listed, so the operator is described as a Middle East operator and the citation stays forthcoming.

The paper describes two steps.

In a September 2025 shop trial, a fabricated 24-inch, Grade X60, 0.5-inch wall joint carried an artificial crack 6 inches long and 50 percent deep. A compression sleeve was dry-fitted, heated to about 400°F (204°C) in about four minutes, tacked, and welded on the long seams. The spool was then pressure-cycled between 36 and 72 percent of SMYS for 10 cycles. After the sleeve was cut off, shear-wave ultrasonic testing and pit-gauge readings showed no crack growth. The draft abstract also describes cyclic testing near 1,800 psi with no leak. The body figures — 36 to 72 percent of SMYS, 10 cycles, no growth — are the ones used here.

On the live line, an ultrasonic crack-detection inspection found a 47 percent deep crack in a seam weld. The compression sleeve on hand was sized for 30-inch pipe and the defect was on a 31-inch section, so the crew shortened the circumference of a conventional 31-inch steel sleeve and dry-fitted it three times. The line was not shut down, and a cut-out was avoided. Crack-growth checks are planned on the next in-line inspection, so the field result is not yet reported.

Figures in the draft, reported here as draft calculations rather than a third-party audit: pipe 31-inch outside diameter by 0.251-inch wall, specified minimum yield strength 52 ksi; sleeve 32.25-inch outside diameter by 0.625-inch wall, specified minimum yield strength 65 ksi; induction target 400°F; line pressure during installation 80 psi; calculated interface pressure about 99 psi after heating, cooling, and internal pressure. The paper’s wording “API PCC-2” is treated as a slip for ASME PCC-2.

## Sources

- [International Pipeline Conference proceedings (paper forthcoming; not hosted)](https://asmedigitalcollection.asme.org/IPC) — ASME