# Coating types

In short. FBE, three-layer polyethylene, coal-tar enamel, tape, and liquid epoxies, described by what they do on a buried line and how they fail.

The coating is the primary corrosion barrier on a buried steel pipeline. Cathodic protection is the second system, for the holidays and the damage. A repair that restores the steel and then leaves the wrong coating, or no coating, has traded a known defect for a new corrosion cell. Part 192 Subpart I and Part 195 Subpart H require external coating on buried or submerged steel, compatible with cathodic protection. They do not name a brand.

**Fusion-bonded epoxy (FBE)** is a plant-applied powder, melted onto a blasted and heated pipe. It is a thin thermoset film. It is also the primer under three-layer systems. Standalone FBE does not shield cathodic protection the way a disbonded polyolefin film can: if it holidays, current can reach the steel. It does not survive a careless backfill, and it needs a field joint coating at every girth weld because the plant coat stops short of the bevel. CSA Z245.20 is the plant-FBE specification widely specified in North America. It is a standards-body document, not a federal rule.

**Three-layer polyethylene (3LPE)** adds a copolymer adhesive and a polyethylene topcoat over an FBE primer. The polyethylene is the handling and rock shield. It is also, if it disbonds and water enters, a shield. Three-layer polypropylene is the higher-temperature version of the same idea. ISO 21809-1 is the international plant-coating standard this family is bought against. The repair question is local: at a dig, do you recoat with a system that matches the plant coat’s service temperature and that does not recreate a shielding flap over the weld.

**Coal-tar enamel** is the historical transmission coating, often with a felt wrap. A great deal of it is still in the ground and still performing. It also cracks, and it is unpleasant and regulated as a material to remove. Recoating a coal-tar cutback with a modern epoxy requires removing the enamel back to a clean edge. Painting epoxy over intact enamel because the enamel “looks fine” is how the new coat lets go at the first holiday.

**Tape**, particularly polyethylene backed tape, is the system the Marshall report tied to disbondment, shielded cathodic protection, and the corrosion-fatigue colony that ruptured Line 6B. Tape is still encountered on older lines and, less defensibly, in a ditch as a quick recoat. ADB-2016-04 generalized the shielding problem to buried insulated coatings. The practical instruction from those two public documents is the same. If the coating can hide wet steel from the cathodic-protection current, the integrity plan has to assume corrosion or stress corrosion cracking under it, and the repair should not put that coating back.

**Liquid epoxies** are the field coatings: two-part materials brushed or sprayed on a prepared weld or a grind. They are only as good as the surface, the mix ratio, the temperature, and the cure before backfill. They are the usual choice for a recoat of modest area and for many field joints. A liquid epoxy specified for atmospheric service is not a buried-pipeline coating. The data sheet’s buried, cathodic-protection-compatible, temperature-rated product is the one the procedure should name.

This note does not rank brands. The specification that belongs in the repair record is the product, the surface-preparation grade that was achieved, the batch, the conditions, and the holiday test. The [field joint note](/coatings/field-joint-coatings) and the [surface preparation note](/coatings/surface-preparation) are the other two halves of that record.

## Sources

- [NTSB/PAR-12/01, disbonded polyethylene tape](https://www.ntsb.gov/investigations/AccidentReports/Reports/PAR1201.pdf) — NTSB
- [ADB-2016-04, shielding and insulated coatings](https://www.federalregister.gov/documents/2016/06/21/2016-14651/pipeline-safety-ineffective-protection-detection-and-mitigation-of-corrosion-resulting-from) — Federal Register
- [49 CFR 192 Subpart I, corrosion control](https://www.ecfr.gov/current/title-49/part-192/subpart-I) — eCFR
- [49 CFR 195 Subpart H, corrosion control](https://www.ecfr.gov/current/title-49/part-195/subpart-H) — eCFR
- [AMPP, publisher of coating and corrosion standards](https://www.ampp.org/) — AMPP