# Pipe and steel basics

In short. Pipe grades, wall thickness, seam types, coatings and cathodic protection, and why the age and make of a pipe change what is safe to do to it.

Before choosing how to repair a pipe you need to know what the pipe is. Two lines with the same diameter can behave very differently if one is modern seamless pipe and the other is older seam-welded pipe with a different coating. This page covers the facts that most often change a decision.

## Grade: how strong the steel is

Line pipe is ordered to a specification, and the specification sets a minimum strength. The grade name usually carries a number. In the common line-pipe grade naming, the number after the letter X is the specified minimum yield strength in thousands of pounds per square inch, so a higher number means a stronger steel. Stronger steel lets a designer use a thinner wall for the same pressure.

Higher strength is not a free upgrade. Some repair products are qualified or tested only for a range of grades. When a repair vendor quotes a grade limit, take it literally.

## Wall thickness

Wall thickness is the second half of the strength story. The pipe spec gives a nominal wall, and real pipe varies from it. Corrosion and grinding remove wall. A repair is often decided by how much wall is left compared with how much the pressure requires. The [corrosion and metal-loss note](/assessment/corrosion-metal-loss/) explains how the remaining strength of corroded pipe is estimated.

Records matter here. For covered segments, the U.S. integrity rules require an operator to gather and integrate pipe data before it evaluates threats. Pipe attributes such as diameter, wall thickness, seam type, joint factor, manufacturer and manufacturing date are listed in [49 CFR 192.917](https://www.ecfr.gov/current/title-49/section-192.917) among the data to integrate. Where the records are missing, the field examination is how the facts get established.

## How the pipe was made: seams

- **Seamless pipe** has no longitudinal weld. It is made by piercing and rolling a solid billet.
- **Welded pipe** is rolled from plate or coil and welded along its length. The seam can be made by electric resistance welding (ERW) or by submerged arc welding. Pipe made by older ERW processes has a documented history of seam problems, covered in [low-frequency ERW seams](/assessment/lf-erw-seams/).
- **Girth welds** join one length of pipe to the next in the field. Every pipeline has thousands of them. See [girth weld and bend repairs](/repair-methods/girth-weld-and-bend-repairs/).

The seam type feeds into a **joint factor** in the design formula, and it tells an inspector where to look for particular kinds of cracks.

## Coatings

Steel in the ground corrodes unless something keeps the soil water away from it. The first defence is the **coating**: a layer applied at the mill and in the field that isolates the steel. Coating types change over decades. Older lines may have tape, asphalt or coal-tar enamels. Newer ones use fusion-bonded epoxy or multilayer polyethylene systems. Each type ages differently, and each one fails in its own way.

Field joints, the bare steel left at each girth weld, get their own coating after welding. They are a common weak point. See [coating types](/coatings/coating-types/), [field joint coatings](/coatings/field-joint-coatings/), and [coating at repair sites](/coatings/coating-at-repair-sites/). A repair that leaves bare steel or a poor coating behind has only moved the problem.

## Cathodic protection

No coating is perfect, so the second defence is **cathodic protection (CP)**. CP puts a small direct current onto the steel, either from a buried block of a more reactive metal (a sacrificial anode) or from a rectifier connected to a groundbed (impressed current). The current makes the exposed steel the cathode of the circuit, which stops it from corroding at coating holidays.

Coating and CP work as a pair. Coating cuts the current that CP has to supply. CP covers the small gaps in the coating. Trouble starts when a coating peels away from the pipe and then blocks the current from reaching the steel. That condition is called shielding. See [cathodic protection](/coatings/cathodic-protection/) for how it shows up at a repair.

## Fittings and components

Pipelines contain more than straight pipe: elbows, tees, flanges, valves and fittings. Their materials and manufacturing quality matter as well. The Canada Energy Regulator has a [page on quality assurance of pipeline fittings](https://www.cer-rec.gc.ca/en/safety-environment/quality-assurance-pipeline-fittings/index.html) that describes why this became a regulatory topic after an investigation noted fittings that did not meet their specified mechanical properties.

## Why this matters for repairs

Five questions come up on almost every job: What grade is the pipe? What is the real wall? What is the seam type? What is the coating? Is the CP working? If the answers are unknown, the [in-ditch examination](/assessment/in-ditch-examination/) is how they get collected.

— The Pipeline Repairs team

## Sources

- [49 CFR 192.3 — Definitions (SMYS)](https://www.ecfr.gov/current/title-49/section-192.3) — eCFR
- [49 CFR 192.917 — Threat identification (pipe attributes, seam type, joint factor)](https://www.ecfr.gov/current/title-49/section-192.917) — eCFR
- [Landowner's Guide to Pipelines (2011), pipe, welding and coatings chapters](https://primis.phmsa.dot.gov/rd/FileGet/7205/Landowners_Guide_to_Pipelines.pdf) — Pipeline Safety Trust, hosted by PHMSA
- [CER Quality assurance of pipeline fittings](https://www.cer-rec.gc.ca/en/safety-environment/quality-assurance-pipeline-fittings/index.html) — Canada Energy Regulator