title: "Composite system types: pre-cured coil, wet lay-up, and pre-preg"
description: "How the three families of pipeline composite repair differ in fiber, resin, cure, fit to bends and fittings, axial reinforcement, underwater use, and what can be inspected after the repair is buried."
section: repair-methods
updated: 2026-11-25
canonical: https://pipelinerepairs.com/repair-methods/composite-system-types/
markdown: https://pipelinerepairs.com/articles/repair-methods/composite-system-types.md
---

# Composite system types: pre-cured coil, wet lay-up, and pre-preg

In short. How the three families of pipeline composite repair differ in fiber, resin, cure, fit to bends and fittings, axial reinforcement, underwater use, and what can be inspected after the repair is buried.

"Composite wrap" covers several different products. They share a job: carry part of the hoop load the corroded or damaged steel can no longer carry. They differ in how the laminate is made, where it can go, and what can go wrong in the field. The [BSEE and PHMSA guideline](https://www.bsee.gov/sites/bsee.gov/files/2023-05/763af.V1.pdf) lists the common parts of any system: a filler (load-transfer) material, typically a two-part epoxy putty; a primer, typically a two-part epoxy; a reinforcing cloth or fiber, typically E-glass or carbon; and a resin that is either applied in the field or pre-impregnated into the cloth.

## The three families

**Pre-cured layered (coil) systems.** Bands of factory-cured composite, usually glass in a polyester or similar matrix, are wound around the pipe in several layers with adhesive between them, over filler in the defect. This was the first composite type to receive a federal waiver for gas-transmission repair, in 1995 (see [official repair guidance](/regulations/official-guidance/)). The laminate's properties are set in the factory, so field variability is mostly in the adhesive, filler, and fit. The coil is made for straight pipe of a given diameter and carries hoop load. It offers little axial reinforcement and does not conform to elbows, tees, or abrupt changes in profile.

**Wet lay-up systems.** Dry fabric is saturated with resin, usually epoxy, on site and wrapped to the designed number of layers. Fabric can be oriented to put fibers in the axial direction as well as the hoop direction, and the laminate conforms to bends, tees, reducers, and girth-weld caps. The cost of that flexibility is that laminate quality is made in the ditch: resin mix ratio, saturation, pot life, ambient and substrate temperature, moisture, and layer count all depend on the crew and the conditions. The guideline stresses pot and working life limits for both the resin and the filler.

**Pre-impregnated (pre-preg) systems.** The cloth arrives with resin already in it. Some systems are activated by water, which is one reason this family is common for wet and splash-zone work. Others need heat. Pre-preg reduces the mixing and saturation variables of wet lay-up while keeping most of its ability to conform to shape.

## Fiber choice

**E-glass** is the most common reinforcement. It is electrically insulating and relatively low in modulus, so the laminate has to strain more than the steel to pick up the same load, which is why glass repairs are usually thicker.

**Carbon** has a much higher modulus, so a thinner laminate can share more load at a given pipe strain. That matters for high-strength pipe, axial and bending loads, and repairs that must limit strain in the steel. Carbon is electrically conductive and noble to steel. Systems that use it are designed with an insulating layer, often glass or an epoxy primer, between the carbon and the pipe.

## Where each fits

| Need | Pre-cured coil | Wet lay-up | Pre-preg |
|---|---|---|---|
| Straight-pipe external corrosion | Common use | Yes | Yes |
| Bends, tees, reducers | No | Yes | Usually |
| Axial or bending reinforcement (girth welds, ground movement) | Limited | Yes, with axial plies | Depends on system |
| Wet or underwater installation | Only systems qualified for it | Only systems qualified for it | Often designed for it |
| Field variability in laminate quality | Lower | Highest | Intermediate |

Every row depends on the system's own qualification, not the family. The [qualification](/codes/composite-repair-qualification/) note covers what the evidence should include. Public case studies on this site show examples of each: [underwater girth-weld corrosion](/case-studies/cs-14-underwater-composite-sleeve-repair-of-girth-weld-corrosion-on-a-12-inch-gas-/), [carbon fiber on a bend](/case-studies/cs-21-carbon-fiber-repair-of-a-deep-crack-on-a-900-mm-gas-transmis/), [an offshore riser](/case-studies/cs-19-composite-repair-of-a-32-inch-offshore-riser-thailand/), and a [coil repair burst-tested after 25 years](/case-studies/cs-16-burst-test-of-a-composite-sleeve-repair-recovered-after-25-years-in-service-/).

## Load transfer and installation pressure

A composite carries load only after the steel strains into it. The filler has to fill the defect completely and be stiff enough in compression to transfer load from the thinned wall into the laminate. If pressure is lowered for installation and raised afterward, the laminate picks up more of the load. The guideline reports that installation pressure up to 50% of SMYS had minimal effect on burst and cyclic performance of composite repairs over corrosion, but that plain-dent repairs installed under higher pressure had significantly reduced fatigue life. PRCI's public abstract on installation techniques addresses the same question for dents.

## After it is buried

Composite laminates are opaque. The steel under them cannot be inspected visually without removing the repair. Most in-line inspection tools still read the pipe wall through a nonmetallic wrap, so continued metal loss can be tracked, but the tools do not assess the laminate itself or its bond. A composite repair record should include enough location data (girth weld references, odometer, GPS) for a later ILI call to be matched to the repair, and the [repair record](/regulations/repair-records/) should state the design life the repair was qualified for.

Composite systems are one option among several. For a comparison with steel sleeves and clamps, see [Selecting a repair](/repair-methods/selecting-a-repair/) and [Composite wraps](/repair-methods/composite-wraps/).

## Sources

- [BSEE and PHMSA composite repair guideline for nonmetallic repairs, January 2018 (PDF)](https://www.bsee.gov/sites/bsee.gov/files/2023-05/763af.V1.pdf) — BSEE
- [PHMSA R&D project 359, selection of pipe repair methods](https://primis.phmsa.dot.gov/rd/projects/359) — PHMSA
- [PHMSA R&D project 658, composite repair guideline](https://primis.phmsa.dot.gov/rd/projects/658/) — PHMSA
- [PRCI public abstract, installation pressure and dent repairs](https://prci.org/report/pr652-184505-r01-evaluating-installation-techniques-for-pipeline-repair-methods/) — PRCI
- [49 CFR 192.713, permanent field repair of imperfections and damages](https://www.ecfr.gov/current/title-49/section-192.713) — eCFR
- [ASME PCC-2 catalog entry](https://www.asme.org/codes-standards/find-codes-standards/pcc-2-repair-pressure-equipment-piping) — ASME