# Composite wraps

In short. What a composite repair reinforces, which standards PHMSA-sponsored guidance treats as the qualification baseline, and why a wrap is not a general leak repair.

A composite repair is a fiber-reinforced polymer wrapped around a prepared pipe so the wrap shares hoop load with the remaining steel. A filler, usually a high-modulus paste, occupies the defect volume so the wrap is not bridging a gap. PHMSA’s repair fact sheet describes the method in one sentence: a fiber wound over a defect, used in place of a Type A sleeve. That sentence is the start of the discussion, not the design.

The load path only exists if three things are true. The defect is not open to the atmosphere in a way the design excluded. The steel surface was prepared to the standard the qualification assumed. And the wrap was built with the thickness, overlap, and cure the design required. The BSEE/PHMSA guideline, written by Stress Engineering Services under a joint contract, is blunt about the alternative: a poorly designed or poorly installed composite does little or nothing.

## What the public research treats as qualified

The same guideline’s recommendations, which apply to the repairs it studied for both offshore and onshore high-pressure pipe, are specific:

- Use a system that has demonstrated compliance with ASME PCC-2, or with ISO 24817, which the report calls the equivalent international standard. PCC-2 Part 4 is the nonmetallic and bonded-repair portion. ISO 24817:2026 is the current edition; the 2017 edition is withdrawn. Neither text is reproduced here.
- Add tests beyond the minimum in PCC-2 when the service needs them: corrosion repairs under cyclic pressure, a duration that represents the design life, the actual environment (including subsea), and external loads such as bending if those loads exist.
- Do not move a system qualified only for corrosion onto another anomaly — plain dents, for example — without performance testing of that anomaly under the loads it will see.

PHMSA research project 359, “Selection of pipe repair methods,” funded long-term pressure and shear tests and cathodic-disbondment work and sat next to the ASME PCC-2 nonmetallic subcommittee. It is a project record, not a product approval list. This site does not rank systems.

PRCI’s long-term composite program (public catalog entry for report PR-201-084504-R01) buried repairs on machined wall loss up to 75 percent of the wall, from several manufacturers, for as long as ten years, with hydrostatic and cyclic pressure while buried. The accompanying public webinar summary is worth reading beside the catalog entry: nondestructive examination found porosity and delamination even in repairs regarded as exemplars, and the burst tests still generally performed. The open question the researchers stated is which of those features are injurious. A clean visual installation record is not a demonstration that the laminate is sound, and a reported indication is not automatically a failed repair.

## Leaks, cracks, and gouges

Composite wrap is a reinforcement. [Section 192.717](https://www.ecfr.gov/current/title-49/section-192.717) does not name it as a permanent leak repair. The performance-based alternative in that section and in [§192.713](https://www.ecfr.gov/current/title-49/section-192.713) is available only when tests and analyses show permanent restoration, and when the operator’s procedure allows the method. Enforcement correspondence in the public PHMSA record has cited operators whose own procedures forbade composite sleeves on leaks, cracks, or weld imperfections, and cited composite repairs of crack-like features that were not ground out. Those are case files, not a regulation that says the word “composite.” They are still the practical reading.

A crack or a gouge is a stress concentrator. Covering it does not remove it. Grinding to sound metal, confirmed by magnetic particle or dye penetrant inspection, is the step the procedures in those cases required before a wrap. Internal corrosion is a different problem again: an external wrap does not stop a pit growing from the inside, and it cannot be inspected from the outside once it is buried except by the in-line tools that can see past the repair.

## Dents and pressure cycling

The 2004 TTO-10 dent study, sponsored by the Office of Pipeline Safety, describes composite reinforcement of a dent as plausible once mechanical damage has been ground out, and as a way to restrain bulging at a dent with corrosion. It also reports that dents continued to move under pressure cycles beneath wraps, and that a wrap is not a permanent repair where pressure-cycle fatigue is the concern.

A later PRCI program, described in the public abstract of PR-652-184505-R01, tested 12.75-inch, 0.188-inch, Grade X42 pipe with plain dents about 3 to 4 percent of the diameter. Repairs were installed at an internal pressure of 64 percent of SMYS and then cycled between 8 and 80 percent of SMYS. Three of fourteen repaired dents reached the 250,000-cycle runout, and those three were steel sleeves. The composite repairs in that series ranged from about 24,000 to about 200,000 cycles. Two companion corrosion repairs with an E-glass wet layup did reach runout. The abstract’s own conclusion is narrow and should stay narrow: installation pressure did not dominate the corrosion repairs they ran, but dent reinforcement installed under pressure needs care, especially on liquid lines that cycle. It is one pipe size and one grade. It is not an allowability table.

IPC2014-33410 is a head-to-head on the same idea, using one E-glass/epoxy system against Type A and Type B sleeves on 12.75-inch X42 pipe. Machined 75 percent wall loss in 0.375-inch pipe burst outside the repair for all three methods, and the hoop strains under the repairs at 72 percent of SMYS were within about 15 percent of each other. Pressure cycling is where the sleeves pulled ahead. At a 36 percent SMYS range the composite failed in the patch at 198,550 cycles; the sleeves were stopped, still intact, at 302,465. Plain dents in 0.188-inch pipe, cycled over a 72 percent SMYS range, failed the composite at 149,913 cycles and left the sleeves intact at 239,897. Using the authors’ factor of 20 and their assumed gas-line cycle rates, that corrosion result is on the order of 30 years and the dent result on the order of 300 years. The test does not travel to another diameter or another pressure spectrum. A circumferential crack is a different load again: axial tension, not hoop stress. The [compression-sleeve note](/repair-methods/compression-sleeves) and the [2026 circumferential-feature summary](/research#ipc2026) are the place for that distinction. A composite qualified only as hoop reinforcement has not been qualified to carry a girth crack.

## Design life is a material input

PCC-2 and ISO 24817 both treat the allowable composite stress as something derived from long-term tests, not from a short-term tensile coupon. Temperature, water, and cyclic pressure knock down the value the designer is allowed to use. A wrap sized for a gas line at modest cycles is not the same laminate as a wrap sized for a liquid line at the same defect depth. The repair record needs the design basis: defect dimensions, design pressure, design life, number of layers, installer qualification, and the surface-preparation standard that was actually met.

That order of work — tensile coupons from a panel (strength, strain to failure, and modulus), then full-scale tests on the defect the system claims — is the sequence the public composite-repair standards describe. It is an account of the order of work, not a finding that any particular laminate passed a particular line. Some systems are offered in an E-glass epoxy form and a carbon epoxy form. Hoop fiber carries corrosion. Axial fiber is what a bend or a girth weld needs, and the 2021 PRCI manual’s appendix treats composite girth-weld repair as use-with-caution: analyze pressure, tension, and bending, and arrange the wrap so a bend failure occurs in the pipe outside it. A starting geometry discussed there is on the order of twice the wall in thickness and about one diameter past the weld on each side, then optimized. That is the manual’s Appendix B, not a cell in B31.4.

Installation pressure is part of the design. IPC2026-185430, by authors at Henkel, Phillips 66, and Acuren, tested a Henkel carbon-fiber system on NPS 12 X42 pipe. The wrap stayed bonded when pressure later fell below the pressure at installation, and burst pressure did not split cleanly with installation pressure until the bare pipe was yielding. Higher installation pressure did raise the mean stress under the wrap. A different resin needs its own test. Length and thickness are the other levers. IPC2026-186007, by TC Energy and Acuren, found more of either lowered steel strain, with diminishing returns, and that an effective-area repair can be shorter than a wrap of the whole indication without changing the acceptance criterion. That argument is for metal loss.

A glass-fiber dent wrap examined in IPC2026-185748, by TBG and CTDUT, had spent six years on a TBG gas transmission line. Shearography did not find damage, and a protected sample was still intact years after removal. One repair, stored out of the weather, is not a design life. The summaries are in the [research library](/research/library/). Plate that is late does not make a wrap legal for a leak. The [selection note](/codes/repair-selection/) is where the codes still say no.

Operator qualification sits underneath the installation. Parts 192 Subpart N and 195 Subpart G require qualified individuals for covered tasks. Whether wrapping is a covered task is a decision in the operator’s written program. Annual manufacturer cards do not replace that program, and the program does not replace a qualified design.

## Further reading

The cycle counts above are summarized, with the citation, on the [research summaries](/research#ipc2014) page. The paper is Alexander, Vyvial, and Wilson, IPC2014-33410, on the [ASME Digital Collection](https://doi.org/10.1115/IPC2014-33410).

Composite repair systems are listed, without a ranking, under [Industry resources](/industry/#composite).

A 2008 EPA Natural Gas STAR presentation treats composite wraps as one alternative that can repair a non-leaking defect without blowing down the line. It is a historical source; the prices in that talk are of that date. The summary is in the [research library](/research/library/#epa-natural-gas-star-2008).

## Sources

- [Composite repair guideline, BSEE and PHMSA (SES report 1461191-PL-RP-07)](https://www.bsee.gov/sites/bsee.gov/files/2023-05/763af.V1.pdf) — BSEE / PHMSA
- [PHMSA R&D project 658 — composite repair guideline](https://primis.phmsa.dot.gov/rd/projects/658/) — PHMSA
- [PHMSA R&D project 359 — selection of pipe repair methods](https://primis.phmsa.dot.gov/rd/projects/359) — PHMSA
- [TTO-10 dent study, November 2004](https://www.phmsa.dot.gov/sites/phmsa.dot.gov/files/docs/technical-resources/pipeline/gas-transmission-integrity-management/65291/tto10dentstudyfinalreportnov2004.pdf) — PHMSA
- [PRCI public abstract — installation pressure and dent repairs](https://prci.org/report/pr652-184505-r01-evaluating-installation-techniques-for-pipeline-repair-methods/) — PRCI
- [PRCI catalog entry — long-term composite repair study](https://research.prci.org/Research/DesignMaterialsConstruction/DMCProjects/MATR-3-34/4675/189067.aspx) — PRCI
- [49 CFR 192.713](https://www.ecfr.gov/current/title-49/section-192.713) — eCFR
- [49 CFR 192.717](https://www.ecfr.gov/current/title-49/section-192.717) — eCFR
- [ISO 24817:2026 catalog entry](https://www.iso.org/standard/86629.html) — ISO
- [ASME PCC-2 catalog entry](https://www.asme.org/codes-standards/find-codes-standards/pcc-2-repair-pressure-equipment-piping) — ASME
- [Alexander, Vyvial, and Wilson, IPC2014-33410, ASME Digital Collection](https://doi.org/10.1115/IPC2014-33410) — ASME
- [Pipeline Maintenance Best Practices: Lessons Learned from the Natural Gas STAR Program (June 2008)](https://19january2021snapshot.epa.gov/sites/static/files/2017-07/documents/june-charlotte-pipeline.pdf) — U.S. Environmental Protection Agency, Natural Gas STAR Program