In short Papers are grouped by the repair question they actually answer. Longer notes on the earlier IPC and PRCI sources stay on the research summaries page. ASME papers from the 2026 conference are cited to the IPC proceedings collection. Individual 2026 paper pages were not posted there when this library was written.
Installation quality and fit
IPC2026-175104 — burst tests with intentional installation flaws
Laughlin, S., and Yap, K. (formerly Enbridge). “Burst Test Validation and Investigation of Repair System Sensitivity to Installation Flaws.” Paper IPC2026-175104. Proceedings of the 2026 16th International Pipeline Conference, Calgary, 21–25 September 2026. ASME.
The program asked whether several installation mistakes at once would knock a laminated, non-welded steel coil sleeve off the short-term survival test in ASME PCC-2 Part 4. One spool was installed as the procedure intended. The other was given dirt, water, adhesive left out of more than one layer, and a deformed coil. For the pipe they used, 72 percent of SMYS was 1,779 psi and the Part 4 design pressure they were measuring against was 2,470 psi. The clean installation burst near 3,700 psi. The flawed one burst near 3,370 psi, less than a 10 percent drop, and both were still above the design pressure. Strain gauges showed the repair engaged the pipe; the flawed spool was slightly less stiff, which the authors tie in part to the missing adhesive. This is one system and one diameter. It is evidence that this architecture had margin against those particular flaws. It is not a finding that a dirty or wet installation is acceptable, and it does not travel to a composite wrap or a welded sleeve.
IPC2026-185430 — installation pressure and a carbon-fiber wrap
Mally, T., Whalen, C., and Duell, J. (Henkel), Zhang, F. (Phillips 66), and Futch, D. (Acuren). “Under Pressure: The Influence of Installation Pressure on Composite Repair Performance.” Paper IPC2026-185430. Same conference.
Most composite qualification spools are wrapped empty. This program wrapped NPS 12, 0.375-inch, X42 pipe, with 3-inch machined notches, at internal pressures that included zero and 72 percent of SMYS, using a Henkel carbon-fiber epoxy system at a fixed test thickness of 12 layers. All three samples burst above 4,000 psig. The wrap stayed engaged when pressure later fell below the pressure at which it had been installed. Higher installation pressure raised the mean stress and moved the onset of yielding in the steel under the wrap to a lower pressure, but burst pressure did not separate in a meaningful way until the bare pipe was yielding. Gauges on the outside of 12 layers still saw strain, so that thickness had not yet made the outer layers idle. The authors say another resin system, or another pipe, needs its own test. The same warning, from a different program, is already on the circumferential-feature summary: a repair installed in the lab at a lower pressure than the field will see extra compression the field joint never gets.
PPIM 2022 — fit-up and the life of a Type B sleeve
Futch, D. B. (ADV Integrity), and Wilson, J. (Allan Edwards). “Effect of Fit-up on Steel Sleeve Life.” Proceedings of the Pipeline Pigging and Integrity Management Conference, Houston, 2–4 February 2022. Clarion Technical Conferences.
Pressure cycling compared a tight-fitting Type B sleeve manufactured by Allan Edwards with a looser sleeve the paper describes only as a different design. The Allan Edwards sleeve lasted. The looser one leaked. The paper does not name the second sleeve. The authors’ reading is that a gap lets a through-wall path pressurize the annulus, and the sleeve then fatigues as a vessel it was not fitted to be. Industry standards still do not set a numerical fit-up gap. The result is a reason to treat fit as a life variable when the sleeve may hold pressure, not as a convenience for the welder.
Composites after they are in the ground
IPC2026-185748 — a wrap removed after years of service
Vicente, T., Beneduzzi, A., and Cardoso, R. (TBG); Mesquita, T., and Souza Filho, B. (CTDUT). “Long Term In Service Performance of Composite Structural Repairs in Pipelines.” Paper IPC2026-185748. Same 2026 conference.
A glass-fiber wrap that had reinforced a dent on a TBG natural-gas transmission line for six years was cut out and examined. Visual shearography did not find damage. A sample kept protected from weather for another twelve years after removal showed no visual, mechanical, or microstructural degradation the authors would call a failure. They argue that standards could treat more dent wraps as permanent. The sample size is this one repair family, stored out of the weather after removal. It does not replace the design-life knockdowns in PCC-2 and ISO 24817, and it does not speak for a wrap left in a wet ditch on a liquid line.
IPC2026-186007 — length and thickness, not a longer wrap by habit
Ganpatye, A., Tomar, M., Turchet, S., and Yu, D. (TC Energy), and Hassanin, A., and Gao, Y. (Acuren). “Optimization of Composite Repairs for Metal Loss Features in Pipelines.” Paper IPC2026-186007. Same conference.
Strain-based finite element work, checked against burst tests, varied composite length at fixed thickness and thickness at fixed length. More length and more thickness lowered the peak strain in the remaining steel, with diminishing returns past a point. Strain in the laminate has to stay acceptable while the steel strain drops. A field case used an effective-area assessment to cover the governing metal loss instead of wrapping the whole indication at full thickness. The acceptance criterion did not change. The repair got smaller. That is a design argument for metal loss. It is not a license to shorten a wrap over a crack or a girth weld, where the load is not the hoop load this study sized.
How a composite system is qualified
A commonly published design sequence for composite repairs matches the public standards’ order of work: coupon the laminate and measure tensile strength, strain to failure, and modulus; choose fiber direction for the load (hoop for corrosion, axial where a bend or a girth weld has to be stiffened); then run full-scale survival tests on the defect the system claims. ASME PCC-2 and ISO 24817 set minimum design tests. They do not make two systems interchangeable. Wet layup can follow oval pipe, elbows, and branches that a steel can cannot. A leak, and many crack-like defects, still need a pressure-containing repair. Plate lead time is an operations problem. It is not an acceptance criterion.
Dents, legacy steel, and odd geometry
IPC2026-184438 — a dent already under a mechanical sleeve
Angles, E., Bratton, J., and Wu, S. (DNV), and Paris, J., Plishka, M., and Haase, J. (Colonial Pipeline). “Assessment of a Dent Previously Repaired With Mechanical Sleeve Utilizing Advanced Finite Element Analysis Methods.” Paper IPC2026-184438. Same conference.
A rock dent from construction, on a Colonial Pipeline river crossing, had been fitted with a mechanical sleeve in 2004. The assessment was done at DNV. The question was whether the dent was still fit and whether the sleeve was holding pressure in the annulus. Three finite-element stories of when the dent was made — before the commissioning hydrotest, after it, or after operations began — were matched to in-line inspection and excavation shape. Damage indicators said cracking during indentation was unlikely, which matched the excavation (no linear indications). Fatigue and a hypothetical crack grown from a shallow starter both gave remaining lives over 100 years in those models, with a factor on life where the dent met a seam. Dent depth versus pressure could not show whether the annulus was full: the inspection pressures were too alike, and a pressurized annulus would hold the depth still. A later inspection at a clearly different pressure would be the useful check. The authors say the same comparison is how to look at an old Type A sleeve when the file does not say whether a hardenable filler was used.
IPC2026-186259 — trepanning windows
Adams, G., Patterson, C., and Chung, M. C. (Stantec), and Eirich, B. (ATCO). “Engineering Evaluation of Trepanning Windows: Use of Finite Element Analysis in Assessment of Unusual Integrity Features.” Paper IPC2026-186259. Same conference.
On a 1949 ATCO gas line that could not be pigged in the ordinary way, a robot found odd features at girth welds. Stantec did the assessment. Excavation showed trepanning windows: construction-era coupons cut out of the weld so the bead could be examined, then patched with a piece of steel that was not necessarily the same thickness or flush with the wall. The practice was obsolete by the 1970s. The patch is a stress raiser, a fatigue starter, and a weld of awkward geometry. It is not a dent and not a metal-loss box, so the usual screening tables do not name it. The paper’s point is the method: build the real geometry, including residual forming stress where it matters, and assess that, rather than forcing the feature into a category it is not. The same habit applies to other one-off construction scars.
Isolation, welding, and hydrogen
IPC2026-185579 — replacing a scraper-trap valve without a shutdown
Alharbi, A., Aqeely, A., Sheikh, M. A., and Alharbi, M. (Saudi Aramco), and Bowie, A., and George, J. “Application of a Tethered Pipeline Isolation Tool for High-Pressure Maintenance Without System Depressurization, Maintaining Production: 56-inch Deployment for a Valve Replacement.” Paper IPC2026-185579. Same conference. The isolation tool in the paper is a STATS Tecno Plug.
A 56-inch scraper-trap isolation valve on a Saudi Aramco sweet crude line was leaking. Sealant injection was treated as temporary. The usual alternatives were a shutdown and a vent, or a hot-tapped bypass. A STATS tethered plug set a double block and bleed in the short spools that were already there, including past drainage rails in the trap, and the valve was changed while the line stayed in service. No extra hot-tap fitting was left on the pipe. The paper’s claim is that the same arrangement can cover other scraper-trap work up to that diameter when the geometry can accept the plug. It is a case record, not a general permission to isolate any line with a tether.
IPC2026-186302 — hydrogen pickup while welding on a hydrogen line
Erxleben, K., Kaiser, S., and Rhode, M. (BAM), and Silvayeh, Z., Taucher, A., and Domitner, J. (Graz University of Technology). “Investigation on Hydrogen Absorption and Diffusion During In-Service Welding on Hydrogen Pipelines.” Paper IPC2026-186302. Same conference. Open Grid Europe ran the welding experiments.
Low-alloy line pipe is often treated as not susceptible to hydrogen embrittlement in ordinary service, at pressures up to about 100 bar and temperatures up to about 60°C. A weld changes that locally. The arc heats the inside surface, and solubility and diffusion rise with temperature. Full-scale welding trials on a pressurized hydrogen pipeline are rarely practical, so the authors used scaled demonstrators from DN 50 to DN 300, walls 4.0 to 7.1 mm, both bright machined pipe and corroded vintage pipe. More heat input and a thinner wall raised the inside temperature and the hydrogen absorbed. A double-pass weld held less hydrogen than a comparable single pass. Oxide on the old pipe acted as a barrier: vintage corroded steel picked up less than new machined steel. After cooling, the simulation put the highest hydrogen between the weld metal and the heat-affected zone, and the single-pass experiment agreed. A related public discussion of welding onto hydrogen and hydrogen-methane lines is Bruce, Boring, Gould, and Huising, PRCI-EFS2023-029, at the 2023 Emerging Fuels Symposium. The in-service welding note is where burn-through and hydrogen cracking sit next to this result.
The sleeve as a formed piece of steel
PPIM 2022 — Bauschinger effect in a rolled sleeve
Futch, D. B. (ADV Integrity), and Wilson, J. (Allan Edwards). “Bauschinger Effect on Rolled Steel Sleeve.” Proceedings of the Pipeline Pigging and Integrity Management Conference, Houston, 2–4 February 2022. Clarion Technical Conferences.
Plate that is coiled, flattened, and then rolled or die-formed into a sleeve half is yielded in more than one direction. The Bauschinger effect is the drop in yield when the next load reverses the previous one. Tensile tests in this program could not separate that drop from ordinary lab scatter. The authors still treat it as reasonable to buy the sleeve plate a little strong: if the design wants 50 ksi yield, ask the mill certificate for about 5 percent more, 52.5 ksi, so the formed sleeve is not quietly under the grade the calculation used. A separate full-scale program, which they cite but do not repeat here, still showed a manufactured sleeve extending the life of a laboratory feature. The 5 percent is their suggestion. It is not a line in Part 192 or Part 195.
There is also no federal manufacturing specification that defines a repair sleeve. Installation rules are plentiful. What arrives on the truck is often qualified only by a visual check and a mill certificate, unless the operator wrote a spec. A half cut from pipe of the same nominal size does not fit over that pipe: the sleeve’s inside diameter is the pipe’s inside diameter, and the carrier’s outside is larger. Closing that gap means extra arc, re-rounding, or a sleeve formed to the carrier outside diameter on purpose. Fit-up trouble on split pipe is geometry, not a crew’s carelessness. Traceability that is actually useful is a heat number tied to a certificate, and a yield number that still means something after forming.
Where the code tables live
The selection logic those papers have to obey is not in the papers. It is in ASME B31.4-2019 Tables 451.6.2.9-1 and 451.6.2.9-2, ASME B31.8S-2018 Table 7.1-1, CSA Z662:19 Table 10.2, and PRCI PR-186-204504-R01 Tables 2 and 3 plus Appendix B on girth welds. Those tables are copyrighted and are not copied here. How they differ, and which table to open for which defect, is on Repair method selection by defect type and code.