Glossary

Terms

Short definitions for the words the notes use. They are not the definitions in a copyrighted standard.

55 terms

3LPE

Also: three-layer polyethylene

A three-layer plant coating: FBE primer, a copolymer adhesive, and a polyethylene topcoat. The polyethylene can shield cathodic protection if the system disbonds and water enters. Three-layer polypropylene (3LPP) is the higher-temperature relative.

Advisory bulletin (ADB)

Also: ADB

A PHMSA notice, published in the Federal Register, that draws operator attention to a safety issue. An advisory bulletin is guidance. It does not, by itself, create a new regulatory duty.

/regulations/advisory-bulletins

Anomaly

A departure from sound pipe, coating, or a weld found by inspection or examination. An anomaly becomes a defect if it fails an acceptance criterion. PHMSA’s July 2026 repair-criteria proposal uses “anomaly” in this broad sense; the current regulations still mix “anomaly,” “imperfection,” and “condition.”

API 579-1 / ASME FFS-1

The fitness-for-service standard. It is organized by damage type (local metal loss, pitting, cracks, dents, and others) and by assessment level. It is used more often on facilities piping than as the line-pipe corrosion method, where B31G and RSTRENG dominate the federal rules.

/codes/api-579

API RP 1160

The recommended practice for managing the integrity of hazardous liquid pipelines. Section 195.452 requires operators’ integrity programs to follow it, in the edition incorporated by reference.

/codes/api-1160

ASME B31.8S

The companion standard to ASME B31.8 on managing gas-pipeline integrity. Sections 192.714 and 192.933 point to its response-timing figure when a condition is not on a special repair list.

/codes/asme-b31-8

ASME PCC-2

ASME’s post-construction repair standard for pressure equipment and piping. Part 4 is the nonmetallic composite-repair portion that PHMSA- and BSEE-sponsored guidance treats as the qualification baseline for composite pipeline repairs.

/codes/asme-pcc-2

B31G

Also: ASME B31G, original B31G

The ASME manual for remaining strength of corroded pipe. The original criterion uses a parabolic metal-loss area, a flow stress of 1.1 SMYS, and a two-term Folias factor limited to L²/(Dt) ≤ 20. It is named, with RSTRENG, in 49 CFR 192.712.

/codes/asme-b31g/assessment/calculators

Barlow formula

The thin-wall expression for hoop stress, σ = PD/(2t), rearranged in 49 CFR 192.105 and 195.106 to a design pressure. Pipeline codes apply it to nominal outside diameter and nominal wall thickness.

/assessment/calculators

Bolt-on clamp

Also: mechanical clamp

A bolted full-encirclement fitting, typically with an elastomer seal. Section 192.717(b)(2) allows a properly designed bolt-on leak clamp when the leak is a corrosion pit. It is not a universal repair for cracks or for every leak.

/repair-methods/bolt-on-clamps

Cathodic protection shielding

A disbonded coating that lets water reach the steel while blocking protective current. Polyethylene tape and some insulated systems are the classic examples in the public record (Marshall; ADB-2016-04).

/coatings/cathodic-protection

Class location

A Part 192 population-density class (1 through 4) that sets the design factor in §192.111: 0.72, 0.60, 0.50, and 0.40 for the basic cases. Class location is a gas-pipeline concept. Part 195 uses a different design-factor structure.

Composite wrap

Also: nonmetallic repair

A fiber-and-polymer system wrapped over a prepared defect, usually with a filler in the defect volume, to share hoop load. Qualification practice is built around ASME PCC-2 Part 4 and ISO 24817. It is a reinforcement method, not a general leak repair.

/repair-methods/composite-wraps

Cut-out and replacement

Removing a cylinder of pipe and welding in new pipe. It is the reference permanent repair in §§192.713 and 192.717 and in the PHMSA repair fact sheet. The replacement and the tie-in welds have to satisfy the design, welding, and testing rules that apply to that line.

/repair-methods/cut-out-and-replacement

Dent

A depression in the pipe wall that changes the curvature. Plain dents, dents on welds, and dents that coincide with metal loss, cracks, or gouges are treated differently. Depth alone is a weak predictor of fatigue life, but the current regulations still use depth and clock position.

/assessment/dents

Design factor (F)

The multiplier in the design formula that keeps design pressure below a fraction of yield. For gas pipe the basic class-location values are in §192.111. For most hazardous-liquid steel pipe, §195.106 uses 0.72, with stated exceptions.

Discovery

In the integrity rules, the moment an operator has enough information to decide that a condition may threaten integrity. The response clock starts then. Both Parts 192 and 195 generally require that determination within 180 days of an assessment unless the operator shows the period is impracticable.

Engineering critical assessment (ECA)

A fracture-mechanics or strain-based analysis used to decide whether a flaw is acceptable for a stated pressure and life. Part 192 uses an ECA for one MAOP-reconfirmation method (§192.632). Dent ECAs are discussed in API RP 1183 and in PHMSA’s 2026 proposal; they are not a blanket substitute for the current dent repair lists.

Epoxy-filled sleeve

A steel sleeve installed with the annulus filled with a structural epoxy so load transfers across the gap and water is excluded. Performance depends on fill quality, surface preparation, and whether the assembly is only a reinforcement or is also sealed as a pressure boundary.

/repair-methods/epoxy-filled-sleeves

ERW seam

Also: electric resistance weld, LF-ERW, low-frequency ERW

A longitudinal seam made by electric-resistance welding. Pre-1970 low-frequency ERW has a wide heat-affected zone and a record of cold welds, hook cracks, and selective seam weld corrosion. Modern high-frequency ERW is a different process. Hazardous-liquid integrity assessments of LF-ERW pipe have to be capable of assessing the seam.

Failure pressure ratio (FPR)

Predicted failure pressure divided by MAOP or MOP. The gas transmission repair rules use thresholds on this ratio (for example, 1.1 for immediate response to metal loss). A ratio of 1.0 means the model predicts failure at the maximum operating pressure.

/regulations/part-192-repair-and-integrity

Flow stress

The stress the remaining-strength methods treat as the point at which the ligament at a defect fails in a ductile steel. Original B31G uses 1.1 × SMYS. The modified criterion uses SMYS + 10 ksi. It is not a specified mill property.

Folias factor

Also: bulging factor

A dimensionless factor, M, that accounts for stress amplification from bulging at a longitudinal metal-loss area. Original B31G and Modified B31G use different approximations of it.

Fusion-bonded epoxy (FBE)

A plant-applied thermoset powder coating fused to a blasted pipe surface. It is the primer layer in many three-layer systems and a common standalone coating. Field joints are coated separately.

/coatings/coating-types

General corrosion

Wall loss over an area, as distinct from isolated pits. Section 192.485 treats pitting so closely grouped that it affects overall strength as general corrosion. Remaining strength is documented under §192.712.

Girth weld

The circumferential weld joining two pipe ends. A cut-out adds girth welds. Metal loss or a dent that interacts with a girth weld is treated more strictly than the same feature in the pipe body.

Gouge

Mechanical removal of metal, usually from excavation or contact damage, often beside a dent. The groove is a stress concentrator. Leaving it under a sleeve or wrap without removing it is a recurring enforcement theme.

/assessment/gouges

Grinding repair

Removal of a shallow crack, gouge, or stress concentrator by grinding, followed by proving that the remaining wall still meets the strength required for the operating pressure, and then recoating. PHMSA’s repair fact sheet describes the limits.

/repair-methods/grinding-and-recoat

High consequence area (HCA)

A location where a pipeline release would have heightened consequences, defined for gas in §192.903 and for hazardous liquids in §195.450. Integrity-management repair schedules apply to covered segments in those areas. Non-HCA gas transmission repair criteria are in §192.714.

Hot tap

A procedure for welding a fitting to a pipe under pressure and cutting into it with a tapping machine. Line plugging (often called stoppling) extends the idea so a section can be isolated without a full shutdown. API RP 2201 is the common industry practice document; it is not restated here.

/repair-methods/hot-tap-and-plugging

Immediate repair condition

A condition the integrity rules require the operator to address at once, usually with a pressure reduction or shutdown until the repair is done. The lists differ for gas HCAs (§192.933), other onshore gas transmission pipe (§192.714), and hazardous-liquid HCAs (§195.452).

In-line inspection (ILI)

Also: smart pig

Inspection of a pipeline from the inside with an instrumented tool. Magnetic-flux leakage tools are the usual metal-loss tools. Crack tools include ultrasonic and electromagnetic-acoustic transducers. Reported depth includes tool tolerance that an assessment has to account for.

Instant-off potential

The pipe-to-soil potential read immediately after cathodic-protection current is interrupted, used to reduce IR-drop error. Part 192 Appendix D requires that voltage drops other than those across the structure-to-electrolyte boundary be considered for the polarized criteria.

/coatings/cathodic-protection

ISO 24817

The ISO standard for qualification, design, installation, testing, and integrity management of composite repairs on piping and pipelines. The 2026 edition is current; the 2017 edition is withdrawn. The standard text is copyrighted.

/codes/iso-24817

Longitudinal joint factor (E)

The multiplier in the design formula for the longitudinal seam. Seamless and modern welded line pipe are typically 1.00. Some older furnace-welded seams are lower. The controlling table is §192.113, and §195.106 points at the same idea.

MAOP

Also: maximum allowable operating pressure

Maximum allowable operating pressure for a gas pipeline. For steel transmission pipe it is established under Part 192 Subpart L, not by the design formula alone. Design pressure from §192.105 is one input.

Mega Rule

Industry shorthand for the gas transmission safety rulemaking that PHMSA split into more than one final rule, notably the 1 October 2019 MAOP-reconfirmation rule and the 24 August 2022 repair-criteria rule. It is not the title of a single regulation.

/regulations/gas-transmission-rules

Moderate consequence area (MCA)

A Part 192 location, defined in §192.3, that is not an HCA but meets a dwelling-count threshold. The 2019 gas transmission rule extended some assessment and MAOP-reconfirmation duties into MCAs.

Modified B31G

A less simplified remaining-strength criterion: flow stress of SMYS + 10,000 psi, an area factor of 0.85, and a three-term Folias factor. It is not the same calculation as RSTRENG effective area.

/codes/asme-b31g/assessment/calculators

MOP

Also: maximum operating pressure

Maximum operating pressure for a hazardous liquid or carbon dioxide pipeline under Part 195. The liquid integrity rules compare predicted burst pressure with MOP, not with a gas MAOP.

Operator qualification (OQ)

The Part 192 Subpart N and Part 195 Subpart G programs under which individuals performing covered tasks must be qualified. Whether installing a particular repair is a covered task is decided in the operator’s written program.

PHMSA

The Pipeline and Hazardous Materials Safety Administration, the U.S. Department of Transportation administration that issues and enforces 49 CFR Parts 190–195.

Recoat

Applying a new coating on a prepared steel surface after a repair or after a failed coating is removed. The repair is not finished while the steel is bare. Field joint coatings are the plant-weld equivalent.

/coatings/field-joint-coatings

RSTRENG

Also: R-STRENG, effective area

The effective-area method developed for PRCI (report PR-3-805), often called RSTRENG. It uses the measured “river-bottom” depth profile instead of a single area factor. 49 CFR 192.712 and 195.452 name it as an acceptable remaining-strength method. This site does not run it.

Selective seam weld corrosion

Also: preferential seam corrosion

Corrosion that attacks a longitudinal seam preferentially, so the flaw behaves more like a crack than like ordinary metal loss. The gas transmission repair rules single out metal loss on certain vintage seam types.

SMYS

Also: specified minimum yield strength

The minimum yield strength the pipe specification requires. Grade X52, for example, has an SMYS of 52,000 psi. Actual yield is often higher. Where records are not traceable, verifiable, and complete, Part 192 requires conservative substitutes under §192.712.

Steel compression sleeve

Also: compression sleeve

A Type A sleeve installed so the carrier pipe under it stays in hoop compression. The 2021 PRCI repair manual discusses it for longitudinal crack-like defects such as SCC, and not for circumferential cracks or field bends. Ends are not welded to the carrier. See the repair-methods note.

/repair-methods/compression-sleeves/research#prci-2021

Stress corrosion cracking (SCC)

Crack colonies driven by a susceptible steel, a tensile stress, and a local environment, classically under a disbonded coating. The Marshall, Michigan, NTSB report is the public reference case for near-neutral SCC under polyethylene tape.

/assessment/cracks/regulations/lessons-from-investigations

Surface preparation grade

Also: SSPC, NACE blast grades

A specified cleanliness of steel before coating, historically written by SSPC and NACE and now published by AMPP. Near-white metal blast (SSPC-SP 10 / NACE No. 2) and white metal (SP 5 / NACE No. 1) are the grades most plant and repair coatings ask for. The visual standards themselves are copyrighted.

/coatings/surface-preparation

Temperature derating factor (T)

The multiplier in §192.105, tabulated in §192.115. It is 1.000 at gas temperatures of 250°F (121°C) or less and decreases at higher tabulated temperatures. Interpolate between rows. Part 195.106 has no T factor.

Temporary repair

A repair installed with a stated life, after which a permanent repair is still required. PHMSA’s temporary-versus-permanent repair FAQs warn against leaving temporary repairs in service as if they were permanent.

/regulations/interpretations-and-faqs

Tool tolerance

The sizing uncertainty of an ILI tool, often applied by adding it to the reported depth before an assessment. A remaining-strength number that ignores tolerance is not a regulatory evaluation.

Traceable, verifiable, and complete (TVC)

The records standard in the gas transmission rules for material properties and MAOP. If the records needed for an analysis are not TVC, §192.607 and the conservative assumptions in §192.712 apply until they are.

Type A sleeve

A full-encirclement steel sleeve whose halves are welded to each other but whose ends are not welded to the carrier pipe. It reinforces a non-leaking defect. It does not contain pressure. See the repair-methods note and ADB-2026-02.

/repair-methods/type-a-sleeves

Type B sleeve

A full-encirclement steel sleeve welded to the carrier pipe at the ends as well as along the side seams, so the sleeve can hold pressure. It is one of the permanent leak-repair methods listed in §192.717.

/repair-methods/type-b-sleeves