05 · Defect assessment
Defect assessment
How corrosion, dents, gouges, and cracks are framed, plus client-side screening calculators.
Hoop stress, design pressure, and B31G calculatorsSteel repair sleeve MAOP tables
Corrosion metal loss
How blunt wall loss is screened with B31G and RSTRENG, what the 80 percent depth limit means, and what the calculator leaves out.
Dents
Plain dents versus dents with metal loss, cracks, or gouges, and why depth thresholds remain in the rules even though depth is a weak fatigue predictor.
Gouges and mechanical damage
Why a gouge is not metal loss, how grinding and the liquid-line 12.5 percent criterion fit together, and what must not be left under a sleeve.
Cracks and crack-like defects
Why metal-loss formulas do not apply, what §192.712 requires of a crack analysis, and how the gas and liquid schedules differ today.
Vintage LF-ERW seams
Why pre-1970 low-frequency electric-resistance-welded seams are a longitudinal-seam threat, how that differs from modern high-frequency ERW, and what an assessment has to be able to see.
Dent engineering critical assessment
The eleven steps §192.712(c) requires before a dent can be cleared by analysis instead of a depth trigger: threats, ILI data, curvature strain, profile change, loads, FEA strain, uncertainty, the 10 percent limits, fatigue with a safety factor of 5, crack growth, and advance notice.
In-ditch examination and ILI verification
What the regulations require once the pipe is exposed: examine and look beyond the excavation, measure what the tool called, validate crack NDE for tight cracks, account for tool tolerance until it is verified, and feed the results back to the tool vendor.