Common defects
In short Corrosion, dents, gouges, cracks and stress corrosion cracking, seam defects, laminations and girth weld problems, with what each looks like and where to read more.
A defect is a flaw in the pipe or a weld that could matter for safety. An anomaly is anything an inspection tool or inspector flags as different from the nominal pipe. Most anomalies are harmless. A smaller number are defects, and a few need action right away. The U.S. integrity rule in 49 CFR 192.917 groups threats into four families: time-dependent (corrosion and cracking that grow with age), stable (flaws from manufacturing, welding or construction that do not grow on their own), time-independent (damage from outside forces such as digging, weather or ground movement), and human error.
Corrosion
Corrosion removes steel. External corrosion happens where soil water reaches the pipe because the coating has failed or been shielded from cathodic protection. Internal corrosion happens when water, deposits or bacteria collect inside the line. Corrosion can be spread thinly over a large area (general corrosion) or concentrated in pits.
The question for any corroded area is how much wall remains and how long and wide the area is. Screening methods and the way they are used are in corrosion and metal loss. Typical repairs are covered in composite wraps, steel sleeves and cut-out and replacement.
Dents
A dent is a local change in the pipe’s round shape, usually from a rock, equipment or a previous impact. A smooth dent by itself may be tolerable. A dent with a gouge, a dent on a weld, or a dent that moves with pressure changes is a bigger concern, because the metal has been worked and can crack under repeated pressure cycles. See dents and dent engineering assessment.
Gouges and mechanical damage
A gouge is metal scraped or gouged out, typically by excavation equipment, leaving a groove and often a hard, cold-worked layer beneath it. The Canada Energy Regulator describes digging without knowing where lines are buried as one of the biggest hazards for pipelines, which is why one-call systems exist. Some damage does not leak at the time and fails later. See gouges. A 2026 conference paper on training staff to identify and respond to unauthorized activities near a line is summarized at IPC2026-185953.
Cracks and stress corrosion cracking
Cracks are the defect type that worries engineers most because they can grow and can fail suddenly. Crack-like defects include fatigue cracks from pressure cycling, cracks at seams and welds, and environmentally assisted cracking. Stress corrosion cracking (SCC) is a family of cracks that form in groups on the outside of the pipe when stress, a susceptible steel and a specific environment under the coating all meet. Section 192.917 names SCC, seam defects, selective seam weld corrosion, girth weld cracks, hook cracks and fatigue cracks as examples of crack-like threats. See cracks.
Seam defects
The longitudinal weld of welded pipe can contain flaws left from manufacturing: lack of fusion, hook cracks, or a weld line that is more vulnerable to corrosion than the rest of the pipe. Older low-frequency ERW pipe and similar vintage seam processes have a long record of seam problems. See low-frequency ERW seams.
Laminations and inclusions
A lamination is a flat internal split in the steel plate, parallel to the surface, created when the steel was made. Many laminations sit in the middle of the wall and do nothing. They become a concern when they run to the surface, lie near a weld, or blister from hydrogen, and when a repair method might change the stress on them. They are usually found by ultrasonic inspection and are judged by their size and position.
Girth weld problems
Girth welds join the pipe sections in the field. Flaws can include cracks, incomplete fusion, and undercut. A girth weld can also be overloaded by bending or ground movement. The Canada Energy Regulator maintains a page on girth weld area strain-induced failures. See also girth weld and bend repairs.
Other things that show up
- Leaks from small holes or fittings.
- Wrinkles and buckles from bending or ground movement.
- Coating damage without any steel loss yet, often found when the pipe is exposed.
- Equipment damage to valves, flanges and fittings.
What to do with this list
Naming a defect is the first step. The next steps are measuring it (how defects are found) and deciding what it needs (how a repair is chosen). For the U.S. gas transmission repair criteria, see 49 CFR 192.714 and the repair schedules summary.
— The Pipeline Repairs team
Sources
Related notes
- Corrosion metal loss — Defect assessment
- Dents — Defect assessment
- Gouges and mechanical damage — Defect assessment
- Cracks and crack-like defects — Defect assessment
- Vintage LF-ERW seams — Defect assessment
- Repair schedules: gas transmission versus hazardous liquid — Regulations and official guidance